Temecula Trusty Concrete

Temecula, CA Hot weather guide

Pouring Concrete in Hot Weather in Temecula

Temecula averages 60 days a year at 90°F or hotter, and fall brings more 100-degree days than summer: 5.5 against 3.2 in NOAA's 1991-2020 normals for the station inside the city. Heat speeds up setting and dries the surface, so a summer or fall pour starts early, is finished fast and is kept wet for days afterward.

60.3 days
A year at 90°F or hotter, and 8.9 at 100°F or more (NOAA normals, 1991-2020).
5.5 vs 3.2
Days of 100°F or more in September to November against June to August.
3 to 7 days
How long a new slab is typically kept curing (NRMCA Concrete in Practice 11).

Last reviewed November 2026.

Pouring concrete in hot weather in Temecula: the numbers

NOAA's nearest climate normals station, USW00053151, is listed as Fallbrook 5 NE but sits inside the Temecula city limits at 33.44 N, 117.19 W, on the south side of town. Its 1991-2020 normals are the best public record of what a Temecula slab goes through: an average high of 76.8°F over the year, August the hottest month at 89.3°F, 60.3 days a year at 90°F or more and 8.9 days at 100°F or more. Those numbers matter most for a concrete driveway in Temecula CA, which sits in full sun, and for the other flatwork on the concrete contractor in Temecula CA page.

Temecula monthly climate normals, 1991-2020
MonthAverage highAverage lowDaily swingRain
January67.5°F47.4°F20.1°F3.17 in
February66.7°F46.4°F20.3°F3.74 in
March70.1°F47.9°F22.2°F2.02 in
April72.1°F50.5°F21.6°F1.00 in
May75.2°F52.9°F22.3°F0.36 in
June80.8°F55.9°F24.9°F0.12 in
July87.2°F60.0°F27.2°F0.08 in
August89.3°F61.8°F27.6°F0.22 in
September87.8°F61.7°F26.1°F0.11 in
October83.1°F58.0°F25.2°F0.70 in
November74.3°F51.9°F22.4°F1.15 in
December67.1°F46.1°F21.0°F2.64 in

Swipe sideways to see every column.

NOAA NCEI U.S. Climate Normals 1991-2020, station USW00053151 (Fallbrook 5 NE, located inside Temecula city limits). Daily swing is the average difference between the day's high and low.

Hot air balloon over the Temecula Valley, with morning fog below the mountains
Morning fog in the Temecula Valley, under a hot air balloon.

Why fall needs as much care as summer

Most people plan around July, but the station's seasonal counts tell a different story. June through August averages 29.1 days at 90°F or more and 3.2 at 100°F or more; September through November averages 26.4 and 5.5. September's average high, 87.8°F, is only 1.5 degrees below August's, and October still averages 83.1°F. Spring, by contrast, has just 4.6 days of 90°F or more from March to May combined.

Hot afternoons, cool nights

Summer days here swing about 27 degrees from high to low; in August the average runs from 89.3°F down to 61.8°F. NRMCA warns that thermal cracking can follow rapid temperature changes, giving a slab placed on a hot day and followed by a cool night as the example. That swing is one more reason to finish early and keep the new slab damp and shaded through its first night.

What heat does to fresh concrete

The industry's definition of hot weather, from the American Concrete Institute's ACI 305R as summarized by the National Ready Mixed Concrete Association, is any combination of high air temperature, high concrete temperature, low humidity, wind and strong sun that hurts the concrete. Each of them speeds up the loss of water from the surface or the chemical reaction that hardens the mix.

  • Concrete sets faster, so the crew has less time to place, screed and finish before the surface stiffens.
  • It needs more water to stay workable. Water added at the truck raises the water-cement ratio and lowers strength and durability.
  • The surface can dry before the concrete sets, which opens plastic shrinkage cracks, more likely with wind above 5 mph and low humidity.
  • Concrete cured hot in its first days ends up less strong later than the same mix cured around 70°F.

How a Temecula pour is planned for heat

None of this rules out a summer driveway. It changes the schedule and the routine on the day, all of it drawn from NRMCA's practice sheets for hot weather and plastic shrinkage.

  • Start early and avoid placing and finishing in the hottest part of the day.
  • Book the trucks so each one can discharge on arrival, with enough crew on site that nothing waits.
  • Ask the ready-mix supplier about water-reducing and set-retarding admixtures; in extreme heat, chilled water cuts concrete temperature by up to 10°F and ice by up to 20°F.
  • Dampen a dry subgrade, the forms and the steel before the pour, without leaving standing water.
  • Put up windbreaks or sunshades, or run a fog spray upwind, when low humidity and wind are forecast.
  • Never sprinkle water on the surface to make finishing easier.

Curing a slab in Temecula heat

Curing starts as soon as the finish is done and typically lasts 3 to 7 days. In a dry climate it matters more than anywhere: NRMCA notes that concrete left in a dry environment can lose as much as half of its potential strength compared with moist cured concrete, and good curing is what reduces crazing, dusting and scaling on the surface later.

Curing methods for outdoor slabs
MethodHow it worksWatch for
Fog spray or sprinklerKeeps the surface continuously wetIt has to stay wet; drying and rewetting is not acceptable curing
Wet burlap or cotton matsHolds water against the slabKeep them wet and weighted down; use materials that won't stain
Spray-on curing compoundSeals water into the slabEven coverage applied right after finishing

NRMCA CIP 11, Curing In-Place Concrete.

When the slab can be used

Concrete Network's guide allows foot traffic after about 24 hours, cars after about seven days, when the slab has reached roughly 70 percent of its strength, and heavy vehicles such as RVs after 28 days. Heat speeds early strength gain, but the timeline is still worth keeping: a corner chipped by a tire in week one stays chipped.

Temecula Valley vineyard rows in winter, with a hilltop winery building and mountains behind
Vineyard rows in winter in the Temecula Valley.

Rain and cold are smaller problems here

The same station records 15.31 inches of rain in an average year, most of it from November to March, with February the wettest month at 3.74 inches. Freezing is close to a non-issue: the normals show 0.2 nights a year at or below 32°F. A winter pour in Temecula is mostly a matter of picking a dry stretch between storms and covering the slab if rain comes early, and on the clay soils described in the Temecula soil guide, keeping that winter water away from the slab edges.

Get a Free Quote

Four quick fields. No charge for the quote.

Hot Weather Concrete in Temecula: Questions

How hot is too hot to pour concrete?

There is no single cutoff. The concrete industry's hot weather guidance, ACI 305R as summarized by NRMCA, treats hot weather as any mix of high air and concrete temperature, low humidity, wind and sun that harms fresh concrete. The practical rule is to avoid placing and finishing in the hottest part of the day, which in Temecula from June into October means an early start.

What is the best month to pour concrete in Temecula?

Spring is the easiest. March through May average highs of 70.1 to 75.2°F at the NOAA station inside the city, with only 4.6 days of 90°F or more across all three months, and rain falls from 2.02 inches in March to 0.36 in May. November is mild too, at 74.3°F, but it starts the rainy season.

Should I water new concrete in hot weather?

Yes, once it is finished, as curing: keep it continuously wet with a fog spray, a sprinkler or wet burlap, or seal the moisture in with a curing compound, typically for 3 to 7 days. NRMCA calls letting it dry and then wetting it again an unacceptable practice, and water should never be sprinkled on the surface to make finishing easier.

Why did my new patio crack the day it was poured?

Probably plastic shrinkage: the surface dried faster than bleed water could replace it, before the concrete set. NRMCA describes these cracks as shallow, roughly parallel, 1 to 3 feet apart and usually stopping short of the slab edge. Wind over 5 mph, low humidity and heat all make them more likely. They are unsightly but rarely weaken a slab.

Does hot weather make concrete weaker?

It can. Hot concrete needs more water to stay workable, and water added at the truck raises the water-cement ratio, which lowers strength and durability. NRMCA also notes that concrete cured at high temperature early on will not be as strong later as the same concrete cured around 70°F.

Planning a summer or fall pour?